Specification and warranty

The specification of the standard TM Hagenboard acacia board, the permitted features of the wood, the warranty terms and the care instructions.

Standard board specification

The boards are supplied as profiles kiln-dried to 12–14 % moisture content, Select & Better grade. Wood density — 760 kg/m³.

Finger-jointed boards are made of blanks from 30 cm to 90 cm long.

The grain is selected so that the tangential cut (annual rings) faces the front side of the board.

12–14 % Moisture content Profiles kiln-dried to their working moisture content.
760 kg/m³ Density Density of acacia wood.
Select & Better Grade Premium grade of timber.
30–90 cm Blanks Length of the blanks in finger-jointed boards.

Tolerances and features of the wood

Acacia is a natural material, so the specification clearly defines which defects are not allowed and which are a natural feature of the species and are permitted on the front and the back of the board.

Not allowed

  • Sapwood
  • Lightning shakes and frost cracks
  • Cracks in any direction / across the grain caused by compression failures
  • Cracks along the growth zones, from load growth or heavy exhaustion of the tree
  • Dead knots, rot
  • Machining chips larger than 5 mm

Allowed on the front side

  • Radial drying checks on the surface or cracks at the board edges, around fixings and around knots
  • Small chips where the grain crosses and at knots (up to 5 mm)
  • Machining chips of no more than 3 mm along the board (but no more than 2 chips per 1 metre of blank)
  • Live knots of all kinds and sizes (a feature of the species)
  • Black knots 2–5 mm in diameter (not through), but no more than 2 per 1 metre of board
  • Deviation from the geometric dimensions on delivery of no more than 2 %
  • Deviation from the nominal length of no more than 2 mm
  • Maximum tolerance at the longitudinal and transverse joints of the board up to 2 mm
  • Boards with impermissible defects of no more than 5 % of a batch

Allowed on the back side

  • Cracks and frost cracks no deeper than ½ of the board thickness
  • Dead knots, sapwood and rot — no more than 2 knots 5 cm in diameter per linear metre and no deeper than ½ of the board thickness
  • Knots and sapwood at the board edges — no more than 1/3 of the board thickness

Boards with impermissible defects — no more than 5 % of a batch.

Warranty

Warranty against rotting of the board — 30 years.

The warranty on coatings and accessories follows the specifications and warranties of their manufacturer.

We provide a warranty for manufacturing and construction defects for the warranty period established by law.

All other defects are excluded from the warranty.

30 years

Warranty against rot

Coatings and accessories — according to the specifications and warranties of their manufacturer.

Please remember!

Wood is a natural product. It reacts differently to weather conditions and temperature changes. We are not responsible for the typical behaviour of wood, which is further amplified by the weather and the environment in which it is used.

Despite careful selection and processing of the material, we cannot completely avoid natural changes in natural wood.

Therefore we cannot accept complaints regarding the following points

Cracking

Drying checks on the surface, end cracks at the board ends, cracks around fixings, as well as cracks at knots and where the grain crosses (where a branch grew).

Dimensional changes

Twisting, bowing, raised grain and linear expansion of the boards at different ambient humidity.

Colour change

UV radiation and rain wash out the colour pigment of the wood, which over time turns the top layer of the boards grey. Depending on the place and conditions of storage, water stains cannot be completely avoided. Organic compounds in plants and iron oxide in water change the colour of the wood from grey-blue to black.

  • Pigmented oil
    Protects the wood from drying out, cracking and soiling and temporarily limits greying.
  • Clear oil
    Does not protect against UV radiation — the surface turns grey over time.
  • 1–2 times a year
    Minimum frequency of treatment with OSMO oil; several times a year when needed.

Care instructions

Water-repellent oil-based coatings with colour pigments protect the wood from drying out, cracking and soiling.

Clear oil does not protect against UV radiation — the surface turns grey. Greying can be temporarily limited with pigmented oil.

We recommend treating the wood with high-quality OSMO oil several times a year, but at least once or twice a year.

Questions about the warranty?

Call or write to us — we will advise you on the specification, warranty terms and board care.